Desmontagem, desengorduramento, despolimento (scotch brite e lixa)
![[Imagem: ACtC-3e-RDQhXWJ15VHg1BqOi4z90N2VchQTEtVB...authuser=0]](https://lh3.googleusercontent.com/pw/ACtC-3e-RDQhXWJ15VHg1BqOi4z90N2VchQTEtVBORUMlMCIvECx2Ege-O5Sv74xVYng8gnTji1r7qeM1qS83aWdIuJAu4HwloSkEhXD-F2WA2hXlKIDmGFcPFYp96Gd7pZqVGTJKflRnI752nui9LkMZ7ps=w2699-h2024-no?authuser=0)
Preparação para levar o promotor de aderência (beta plast) um primário Epoxy (Upol Raptor, 2 componentes)
![[Imagem: ACtC-3fmQ6dgJU0ksTDuflkhAwxw6sw6Fu-TfaRj...authuser=0]](https://lh3.googleusercontent.com/pw/ACtC-3fmQ6dgJU0ksTDuflkhAwxw6sw6Fu-TfaRj190iZWz_sIUmHK9ugVxxt0UPAbe7rF3HEUj9OkyXnT8SBBoH3cGurAoHQWC50s7sRj0NSajkPTTHW9W7MdQGB7nnQsSWn5Omq-XTZ6u1qxD46TbuS5ck=w2699-h2024-no?authuser=0)
Cura do primário epoxy com infravermelhos de onda curta
![[Imagem: ACtC-3ddTfeKzpwk82llAwAslV09FkcvTGoo1Isa...authuser=0]](https://lh3.googleusercontent.com/pw/ACtC-3ddTfeKzpwk82llAwAslV09FkcvTGoo1Isa-FVHeDx2Qsv18hUz8CphuUG4RqrsYd6NXNNVJqSgLYdoJ8JvAukzNy0jMJCq1ATR8gEa8o0NfTofAuoNDcibytbf6G8Muq7uOpvx8htPIuB_90wxEzVl=w1519-h2024-no?authuser=0)
Aplicação de poliéster para plásticos (dinitrol) por cima do epoxy
![[Imagem: ACtC-3eLWaBJN7anf6Vb7XRLPzXOEEuzo56Slxs3...authuser=0]](https://lh3.googleusercontent.com/pw/ACtC-3eLWaBJN7anf6Vb7XRLPzXOEEuzo56Slxs32RkbgB4C2VgGHtoIHr24dVEoQ9jjIEbaySH_tcQaOZ_pz93owgFnO7hQss_3tZeCmHApkY3xKAlW41ahGfO5MMQcgQBTy87RO_rwdNauxssLcptAo8Pt=w2699-h2024-no?authuser=0)
Nova aplicação de epoxy e despolimento do epoxy:
![[Imagem: ACtC-3eu5uWCzinG1fetv9t2e1uUbf3cl-k_NuL6...authuser=0]](https://lh3.googleusercontent.com/pw/ACtC-3eu5uWCzinG1fetv9t2e1uUbf3cl-k_NuL6OCewKU1lZF5ilQiXKD8IPy70vgsaJMm38bgpnIBns3_Gm5q1HHjnUseUoDqZj9l05s7mqMdDOwAhnf4PutwNA4OqpzxvAyPV7DbDNUO9gkyp8jkepJ3S=w2699-h2024-no?authuser=0)
Tinta acrílica cinzenta:
![[Imagem: ACtC-3fJKeFeXuuhOCFR1ac8JGCUSxHSUBw8DKdH...authuser=0]](https://lh3.googleusercontent.com/pw/ACtC-3fJKeFeXuuhOCFR1ac8JGCUSxHSUBw8DKdH6H3qLfxhK_A9vipeE0LuhiKHi-USomREAtbuNhcIb2vEbZj9NHfxPtg3D2hgqxnKLwHQBw69FYvgEW3IfvJgE0P4VI1WBkZTCjZADSMo_veuuswUhsld=w2699-h2024-no?authuser=0)
Verniz uretano de 2 componentes (barato!)
![[Imagem: ACtC-3eQB4eShXBkKEH65irrxnE-l4bJw41svf8q...authuser=0]](https://lh3.googleusercontent.com/pw/ACtC-3eQB4eShXBkKEH65irrxnE-l4bJw41svf8q88KVJG4913gksJTEsvAgs_0YzSWQgQemuPMYUWYr8O94X9A4DEG9m_po5WjZhZ3KTbIFUptwSzkQ_NcCUcn0-Qc69vewriK7ialz9nE2MwfaXhWSSCgT=w2699-h2024-no?authuser=0)
Aspecto final
Preparação para levar o promotor de aderência (beta plast) um primário Epoxy (Upol Raptor, 2 componentes)
Cura do primário epoxy com infravermelhos de onda curta
Aplicação de poliéster para plásticos (dinitrol) por cima do epoxy
Nova aplicação de epoxy e despolimento do epoxy:
Tinta acrílica cinzenta:
Verniz uretano de 2 componentes (barato!)
Aspecto final
PS: espero não ter ofendido ninguém.